Description
Uses
heavy construction; house fran1ing; posts; spars; lock gates; marine construction in fresh and salt water
Wood Description
Sapwood | distinct, yellow-brown |
---|---|
Heartwood | red-brown, somewhat striped or flame-like figured |
Grain | straight, sometimes slightly interlocked |
Texture | fine |
Remark | – |
Technological Characteristics
Physical properties | |
---|---|
Green density (g/cm³) | – |
Air-dry density at 12% (g/cm³) | 1.17 |
Basic specific gravity | – |
Total tangential shrinkage (%) | 9.5 |
Total radial shrinkage (%) | 5.9 |
Total volumetric shrinkage (%) | – |
Processing
Sawing | Power required y |
---|---|
Blunting effect | Â High (silica) |
Drying | Air-drying easy when dried at a moderate rate |
Machining | difficult because of hardness and sillca content; special tools recommended |
Gluing | – |
Nailing | Pre-boring necessary |
Finishing | – |
Veneering | – |